Skip to content
Ok-Go Packaging

Strength and testing

How heat and humidity weaken corrugated boxes

By Ok-Go Packaging team· Reviewed by Plant management· Updated

Quick answer

Moisture, more than heat itself, is what weakens corrugated. Paper soaks up water from humid air, and published loss factors show a box under load keeps about 80% of its compression strength at 70% relative humidity, 68% at 80% and 48% at 90%, compared with the same box at 50%. Humidity that swings up and down does more damage than steady air.

A corrugated box is paper, and paper trades moisture with the air around it. When the air gets more humid, the board takes on water, and wet fibers carry less load. That is why the same box that stacks fine in a dry warehouse can lean or crush in a humid one, without anything else changing.

Why does humidity weaken corrugated boxes?

The amount of water in board follows the relative humidity (RH) of the air around it. Georgia Tech’s Renewable Bioproducts Institute gives a simple relationship for unbleached kraft linerboard: moisture content rises about 1.35 points for every 10 points of RH. More moisture means less compression strength in the paper, then in the board, then in the box.

The same work gives a rule of thumb buyers can use: around the standard lab condition, a 10-point change in RH changes compression strength by roughly 10%. Lab tests are run on board conditioned to a standard atmosphere (TAPPI T 402) for exactly this reason. A box tested in the lab and a box sitting on your dock in August are not at the same humidity.

How much strength does a box lose at each humidity?

The figures most often used come from the Fibre Box Association’s loss factors, credited to the USDA Forest Products Laboratory and reproduced by Georgia Tech. They describe a box under load, compared with the same box at 50% RH.

Compression strength a box keeps at each humidity Box under load, compared with the same box at 50% RH 50% RH 100% 60% RH 90% 70% RH 80% 80% RH 68% 90% RH 48% 100% RH 15% Source: FBA loss factors credited to USDA FPL, via Georgia Tech
Strength kept under load at each humidity, compared with 50% RH. Source: FBA loss factors credited to USDA FPL, via Georgia Tech.
Relative humidity Approx. board moisture (unbleached kraft) Compression strength kept
50% about 7% 100%
60% about 9% 90%
70% about 10% 80%
80% about 11% 68%
90% about 13% 48%
100% about 14% 15%

The moisture column is calculated from the Georgia Tech relationship for one paper type; your board will differ somewhat. The strength column is the published factor. Note the curve: going from 80% to 90% RH costs far more than going from 50% to 60%.

Swings make it worse. The loss factors carry a warning that cycling humidity increases the loss, and Forest Products Laboratory research found that cyclic humidity changes significantly reduce the strength of paperboard under compressive load. A box that goes from a humid dock to a dry office and back every day is worse off than one that sits at a steady 70%.

What about heat?

The published loss factors are written in terms of humidity, not temperature. Heat matters to a box mainly through what it does to the moisture around it:

  • Cold loads sweat. Product or boxes coming out of a cooler into warm, humid air can collect condensation on their surfaces, which wets the board directly.
  • Cold rooms are humid. Georgia Tech describes refrigerated warehouses as high-humidity environments; in one case, heavy single-wall board stored at 4 °C (39 °F) and 80% RH reached about 12% moisture.
  • Hot, dry storage dries board out. Dry board is stronger in compression, but very dry board can crack along score lines when it is folded, especially heavy grades.

What does this mean in El Paso and the Southwest?

Our region is dry most of the year, which is easy on stored boxes. The risk comes from short, local moisture events that a spec written for “dry climate” can miss:

Situation What happens to the board What to do
Summer monsoon storms Humidity jumps for hours or days; open dock doors let wet air and rain in Keep stock away from doors, cover pallets, don’t stage boxes outside
Evaporative (swamp) coolers These coolers work by adding moisture to the air, so the space near them runs humid Store boxes and loaded pallets away from cooler outlets
Long warehouse storage Time under load and humidity losses stack on top of each other Stack in columns, rotate stock, size the grade for the longest storage
Produce coolers and cold storage High humidity plus condensation when loads move out Spec for the cold room, not the plant floor; consider moisture-resistant board
Hot trailers and yards Board dries out; scores can crack on fold Fold carefully, store flat boxes inside before use

How do you spec a box for humid conditions?

Start by telling your supplier where the box will actually live: the worst humidity it will see and for how long. Then choose from the usual ways to compensate, which Georgia Tech lists as heavier board, wet-strength additives or adhesives, and surface barrier coatings:

  1. More compression strength. A higher ECT grade or double-wall, sized with a humidity safety factor so the box still has enough compression strength at your worst RH. Our guide to box compression and stacking strength shows the math.
  2. Moisture-resistant treatments. Water-resistant coatings and wax slow the board’s water uptake. They are not waterproofing; see are corrugated boxes waterproof? for what each option can and can’t do.
  3. Better storage. Columns instead of interlocked stacks, nothing on bare floors, oldest stock first. If you don’t have room to store boxes well, a stocking program lets the supplier hold inventory and release it on your schedule.

We make moisture-resistant boxes and standard shipping boxes, and we run stocking programs from our own warehouse space in Socorro.

Common questions

Does humidity really weaken cardboard boxes?

Yes. Corrugated is made of paper, and paper absorbs moisture from the air. Published loss factors for boxes under load show about 20% of compression strength gone at 70% relative humidity, 32% at 80% and 52% at 90%, compared with 50% humidity.

Is desert heat bad for corrugated boxes?

Dry heat on its own is not the main problem; dry board is actually stronger in compression. The trouble in desert climates comes from moisture events: monsoon storms, evaporative coolers, wet pallets and cold loads sweating on a warm dock. Very dry board can also crack along score lines when it is folded.

How should I store boxes in a humid warehouse?

Keep them off the floor and away from dock doors and coolers, use the oldest stock first, keep stacks in columns, and avoid leaving loaded pallets in the stack longer than needed. If high humidity is normal for your building, design the box for it with a stronger grade or a moisture-resistant treatment.

Do wax or water-resistant coatings stop strength loss?

They slow down how fast water gets into the board, which helps with wet surfaces and short exposures. How much strength they hold in long, humid storage depends on the treatment, so ask for test results at your conditions rather than assuming a coated box behaves like a dry one.

Sources

  1. Effects of Moisture Content on Box Compression Strength: FBA BCT Loss Factors (R. E. Popil, 2018, updated 2019), Georgia Tech Renewable Bioproducts Institute. Accessed November 25, 2026.
  2. Measuring the mechanical behavior of paperboard in a changing humidity environment (Gunderson and Considine, 1986), USDA Forest Service, Forest Products Laboratory. Accessed November 25, 2026.
  3. Standard conditioning and testing atmospheres for paper, board, pulp handsheets, and related products, T 402 sp-26, TAPPI. Accessed November 25, 2026.

Have a box in mind? Send us the dimensions, weight and quantities and we will quote it.

Products for this job

Related guides

Glossary terms in this guide

About the author

Ok-Go Packaging team · Quality control

CallGet a quote