Quick answer

ECT (edge crush test) measures how much load corrugated board carries when it is pressed on its edge, so it predicts how well a box stacks. The Mullen (burst) test measures the pressure it takes to break through the flat board, so it relates to punctures and rough handling. If your boxes are palletized and stacked, specify ECT; a burst rating still earns its place for heavy, dense or roughly handled contents.

ECT and Mullen are two lab tests on the same corrugated board, and they answer different questions. ECT tells you how the board behaves standing on edge in a box wall that is holding up a stack. The Mullen test tells you how hard you have to push on the flat board before something breaks through it. Most shipping boxes spend their life in stacks (on pallets, in trailers, in warehouses), which is why ECT is the rating most buyers should start with.

What does the edge crush test (ECT) measure?

ECT is the force a short strip of corrugated board can carry, standing on its edge, before it crushes. The lab method is TAPPI T 811, also called the short column test, and it covers single-, double- and triple-wall board. The freight rule that governs box certificates describes it the same way: the sample stands upright with the flutes running in the direction of the load, and the result is reported in pounds per inch of width. A 32 ECT board held 32 lb for every inch of edge before it failed.

That is exactly how a box wall is loaded at the bottom of a stack, so ECT is the input for estimating how much a box can carry. Our guide to box compression and stacking strength shows how ECT turns into a box compression estimate.

Edge crush test (ECT) Flutes stand up, load on edge A short strip is crushed on its edge Result: lb per inch (e.g. 32 ECT) Predicts stacking strength Mullen burst test Diaphragm pushes up Flat board is pushed until it bursts Result: psi (e.g. 200 lb test) Relates to punctures, rough handling
ECT crushes the board on its edge, the way a stacked box wall is loaded. Mullen pushes through the flat face.

What does the Mullen (burst) test measure?

The Mullen test clamps a piece of flat board over a rubber diaphragm and pumps hydraulic pressure under it until the board ruptures. The peak pressure, in pounds per square inch, is the bursting strength. TAPPI T 810 is the method for single-wall and double-wall board in the 100 to 700 psi range; it isn’t used on triple-wall, which freight certificates rate with a puncture test instead.

A “200 lb test” box is one whose board burst at 200 psi or more. Because burst strength depends mainly on the liners, a burst-rated freight certificate also states a minimum combined weight of the facings: the liner basis weight, in pounds per 1,000 square feet.

When does ECT matter more, and when does Mullen?

Pick the rating that matches how your box is most likely to fail.

Situation Rating that matters most Why
Boxes stacked on pallets, in trailers or in racks ECT The bottom boxes carry everything above them, on edge
Long storage, humid docks or cold rooms ECT, with extra margin Compression strength drops with time under load and with humidity
Heavy, dense or hard-edged contents (castings, fasteners, hardware) Burst helps The product presses on the panels and can punch through
Boxes handled one at a time and dropped Both Drops load the panels; the box still gets stacked at every stop
Jumbo boxes and bulk bins ECT, plus structure Walls carry the load above; pads, sleeves and partitions add support

If nobody (your customer, a retailer or a freight requirement) names a rating, ask yourself what has gone wrong before. Crushed bottom boxes and leaning pallets point to ECT. Torn corners and holes punched by the product point to burst strength or a heavier liner.

How do ECT and Mullen ratings line up?

The most useful published pairing comes from the freight rule itself. NMFC Item 222 lets a box maker certify a box either by burst test (with a minimum liner weight) or by ECT, and its text names the ECT value it accepts in place of a burst value. These pairs appear in the 2025 edition of the rule (NMF 100-AY01):

Wall Burst test ECT the rule accepts instead
Single-wall 175 lb 29 ECT
Single-wall 200 lb 32 ECT
Single-wall 275 lb 44 ECT
Double-wall 200 lb 42 ECT (same 80 lb and 85 inch limits in the rule’s certificate examples)
Double-wall 275 lb 48 ECT

Treat these as freight-rule alternatives, not lab conversions. A 32 ECT board and a 200 lb test board both qualify a single-wall box for the same weight and size limit, but they are built differently and will behave differently. If you are switching an existing spec from burst to ECT, run the new box with your product before you change the whole order.

Why are ECT-rated boxes often lighter?

Compare the two certificates. A burst certificate lists a minimum combined liner weight (84 lb per 1,000 sq ft on the rule’s single-wall 200 lb example). An ECT certificate has no liner-weight line at all. The box maker only has to prove the board actually tests at the stated ECT, so it can choose the combination of liners and medium that gets there. That can mean lighter board for the same stacking performance.

The trade-off: lighter liners can mean less puncture resistance. If your product has sharp edges or concentrated weight, keep a burst requirement or a minimum liner weight in the spec.

Which rating should you put on your spec?

  1. If your customer, a retailer or a freight requirement names a rating, use it exactly as written.
  2. If the box will be stacked (most will), specify ECT and tell your supplier how it will be stacked: how high, for how long and in what humidity. Our article on how heat and humidity weaken boxes explains why that last part matters.
  3. If the product is heavy, dense or sharp, add a burst requirement or a minimum liner weight.
  4. Check the wall construction too. Going from single-wall to double-wall changes both numbers more than small grade changes do; the flute guide covers the options.
  5. Pack and test a real sample before committing to a production run.

The rating you choose is printed in the box maker’s certificate; how to read a box maker’s certificate walks through every line. The test methods behind both ratings are published by TAPPI.

At Ok-Go we cut samples on our own sample table within hours, so you can pack, stack and drop your real product in the real box before you approve a shipping box or a jumbo box for production.

Common questions

Is 32 ECT the same as 200 lb test?

They are accepted as alternatives, not as equals. The freight rule (NMFC Item 222) lets a single-wall box certified at 32 ECT or at 200 lb burst carry the same limits: 65 lb gross weight and 75 united inches in the rule's own certificate examples. But the two tests measure different things, so a 32 ECT board won't necessarily burst at 200 psi, and a 200 lb test board won't necessarily crush at 32 lb per inch.

Is a higher Mullen box better for stacking?

Not reliably. Burst strength depends mainly on the liners, while stacking strength depends on how the whole board resists crushing on edge. If stacking is the job, compare ECT values, or better, compression-test the finished box.

Can a box have both an ECT and a Mullen rating?

The board can be tested both ways, but the circular freight certificate printed on a box states one test: burst (with a minimum combined liner weight) or edge crush. If your spec needs both numbers, write both on the spec and ask your supplier for test results.

What do 44 ECT and 48 ECT mean?

The board held 44 or 48 pounds of force per inch of edge in the edge crush test before it failed. In the freight rule's text, 44 ECT is the single-wall alternative to 275 lb burst, and 48 ECT is the double-wall alternative to 275 lb burst.

Sources

  1. Edgewise compressive strength of corrugated fiberboard (short column test), T 811 om-23, TAPPI. Accessed November 25, 2026.
  2. Bursting strength of corrugated board, T 810 om-22, TAPPI. Accessed November 25, 2026.
  3. NMFC Items 222-1 to 222-6 and 299, Specifications for Fiberboard Boxes (reproduced from NMF 100-AY01, 2025), National Motor Freight Traffic Association, via Fibre Box Association. Accessed November 25, 2026.

Have a box in mind? Send us the dimensions, weight and quantities and we will quote it.

Products for this job

Related guides

Glossary terms in this guide

About the author

Ok-Go Packaging team · Quality control

CallGet a quote